Dependence of restoration stability from post-cure after matrix system replacement (laboratory test)

Authors

  • D.Yu. Fadeeva 1, аспирант кафедры гериатрической стоматологии
  • V.N. Chilikin 1, д.м.н., заслуженный врач РФ
  • T.V. Greniv 2, директор по качеству и разработкам
  • 1 МГМСУ им. А.И. Евдокимова
  • 2 ЗАО «СтомаДент»

Abstract

The restoration of class II cavities always requires using of matrix system. Generally, in the directions for use of materials is not specified the need of further restoration polymerization after matrix removal from the vestibular and oral surfaces. Some doctors give additional curing, some do not. Evidence-based medicine does not provide any recommendations about that. Inadequate curing time can lead to incomplete composite polymerization, in consequence of which fragmentary restoration chipping may occur.

Key words:

class II, the additional polymerization, matrix system, fragmentary chipping, direct restoration, contact point

For Citation

[1]
Fadeeva D.Yu., Chilikin V.N., Greniv T.V. Dependence of restoration stability from post-cure after matrix system replacement (laboratory test). Clinical Dentistry (Russia).  2015; 2 (74): 8—9

References

  1. Чиликин В.Н. Новейшие технологии в эстетической стоматологии. - М.: Медпресс-информ, 2007. - С. 70-71.
  2. Николаев А.И., Цепов Л.М. Как повысить эффективность лечения кариеса зубов. - Клиническая стоматология. - 1998; 2: 32-6.
  3. Rau P., Pioch T., Staehle H-J. Influence of rubberdam on proximal contact strengths. - Int poster J Dent Oral Med. - 2005; 7 (7): 271.
  4. Мангани Ф., Пцтиньяно А., Черцтти А. Руководство по адгезивной стоматологии: ключевые аспекты успешной реставрации. - Квинтэссенция. - С. 136.
  5. Макеева И.М. Восстановление зубов светоотверждаемыми композиционными материалами. - М.: Стоматология, 1997. - С. 71.
  6. Kurtzman G.M. Improving proximal contours for direct resin restoration. - Dentistry today. - 2010; 29 (4): 108-9.

Published on

June 1, 2015